• HDPE Geomembrane for Wasterwater Treatment Lagoons
  • HDPE Geomembrane for Wasterwater Treatment Lagoons
  • HDPE Geomembrane for Wasterwater Treatment Lagoons
  • HDPE Geomembrane for Wasterwater Treatment Lagoons
  • HDPE Geomembrane for Wasterwater Treatment Lagoons
  • HDPE Geomembrane for Wasterwater Treatment Lagoons

HDPE Geomembrane for Wasterwater Treatment Lagoons

Certification: CE, ISO
Surface: Smooth
Application: Transportation Project, Hydraulic Project, Geotechnical Project, Environmental Project
Feature: Puncture Resistance, Impact Resistance, Tear Resistance
Material: HDPE
Color: Black
Samples:
US$ 0/Square Meter 1 Square Meter(Min.Order)
| Request Sample
Customization:

Contact Supplier

Diamond Member Since 2012

Suppliers with verified business licenses

Basic Info.

Model NO.
Elite-Membrane
Product Name
HDPE Geomembrane
Raw Material
Virgin/ Recycled HDPE
Function
Antiseepage and Separation
Thickness
0.2mm-2.5mm
Width
1m to 8m
Length
Normal 50m/100/M or as Per Your Request
Color 1
Normal Is Black or as Per Your Request
Test Method
ASTM D Standard
Certificate 1
ISO
Certificate 2
CE
Transport Package
Thickness 1mm, 5.8mx50m Per Roll, 19140m2/20′gp
Specification
CE
Trademark
elite-indus
Origin
Anhui
HS Code
39219090
Production Capacity
40000m2/ Day

Product Description

HDPE Geomembrane Wasterwater Treatment Lagoons

HDPE Geomembrane Introduction:
 
EltMembrane-GH series of geomembrane is manufactured from High Density Polyethylene resins. The surfaces of both sides are smooth.the products are manufactured by the technology of coextrusion-blown triple layer.

HDPE Geomembrane Performance:
 
1, Excellent physical and mechanical performance, high tearing resistance;good deformation adaptability, high puncture resistance;
2, High aging resistance, high UV resistance, anti-acid & alkali;
3, Excellent low & high temperature resistance, innocuous, long life span;
4, Perfect water proof performance, seepage and humidity resistance. 
 
HDPE Geomembrane Application:

1,Prevent leakage disposal in landfill or waste water or waste dregs disposing field. 
2,River bank, lake dam, mine remainings, reservoir, tunnel. Liquid storage pool(pit, mine) 
3,Preventing leakage in subway, basement, tunnel, hole. Anti-salt leskage in roadbed and other groundsill. 
4,The plane direction laying of dam, the vertical direction laying for groundsill, used in the construction fence and waste material field. 
5,Used in seawater of freshwater feed field. 
6,Used in groundsill of road, highway, railway and waterproof layer of swelling clay and wet collapsed loess. 
7,Preventing leakage on rooftop
 
HDPE Geomembrane Technical specifications
 
1) GH standard
NO. Item Index
GH-HDPE
        GH-1  GH-2 
1 The tensile strength Mpa ≥ 17 ≥ 25
2 The percentage of breaking elongation rate % ≥ 450 ≥ 550
3 Right-angle tear strength N/mm ≥ 80 ≥ 110
4 Carbon black content 13% ≥ 2
5 Environmental stress cracking resistance F 20h - ≥ 1500
6 Oxidative induction time at 200 ºC min - ≥ 20
7 The permeability coefficient of water vapor ≤ 1.0 × 10 -13
gcm/(cmsPa)
8 The impact and embrittlement property in low-temperature at 70 ºC below zero pass the detection
9 Dimensional stability percentage % ± 3

2) ASTM D Standard
No. Properties Test Method Test Value
1 Thickness(mm) ASTM D5199 0.50 0.75 1.00 1.25 1.50 2.00 2.50 3.00
2 Density (g/cm2) ASTM D1505   0.939
3 Tensile Propeties    
Yield Strength(N/mm) ASTM D6693 7 11 15 18 22 29 37 44
Break Strength(N/mm) 13 20 27 33 40 53 67 80
Yield Elongation % Type IV 12
Break Elongation %  700
4 Tear Resistance/N ASTM D1004 62 93 125 156 187 249 311 374
5 Puncture Resistance/N ASTM D4833 160 240 320 400 480 640 800 960
6 Stress Crack resistance/hr ASTM D5397
(App.)
300
7 Carbon Black   
Carbon Black Content % ASTM D1603 2.0-3.0
Carbon Black Dispersion ASTM D5596 Carbon black dispersion(only near spherical agglomerates)
for 10 different views 9 in categories 1 or 2 and 1 in category 3
8 Oxidative Induction Time(OIT)  
Standard OIT/min ASTM D3895 100
High Pressure OIT/min ASTM D5885 400
9 Oven Aging at 85°C  
Standard OIT-% retained after 90 days    ASTM D3895 55
High pressure OIT-% retained after 90 days    ASTM D5885 80
10 UV Resistance  
Standard OIT retained 
after 1600 hrs
ASTM D3895 50
High pressure OIT retained 
after 1600 hrs
ASTM D5885 50
11 Low tempreture impact
 brittle property at -70°C
_ Pass
12 Permeability g·cm/(cm2)·Pa _ ≤1.0×10-13
13 Dimensional Stability/% _ ±2
High Density Polyethylene Plastic Geomembrane

1, Smoth surface HDPE Geomembrane
2, Textured surface HDPE Geomembrane
3, HDPE anti-skid point Geomembrane


HDPE Geomembrane Usage:

1, Prevent leakage disposal in landfill or waste water or waste dregs disposing field.
2, River bank, lake dam, mine remainings, reservoir, tunnel. Liquid storage pool(pit, mine)
3, Preventing leakage in subway, basement, tunnel, hole. Anti-salt leskage in roadbed and other groundsill.
4, The plane direction laying of dam, the vertical direction laying for groundsill, used in the construction fence and waste material field.
5, Used in seawater of freshwater feed field
6, Used in groundsill of road, highway, railway and waterproof layer of swelling clay and wet collapsed loess.
7, Preventing leakage on rooftop

Geomembrane Catergory:

Geomembrane including LDPE, LLDPE geomembrane, HDPE geomembrane, EVA geomembrane, ECB geomembrane, PVC geomembrane geomembrane with textured surface.
                     HDPE Geomembrane specifications (CJ/T234-2006)(USA GRI-GM13 Standards)
NO. Value(mm) 0.75 1.00 1.25 1.50 2.00 2.50 3.00
1 Density (g/cm3) 0.939
2 Tensile propeties              
  Yield strength(N/mm) 11 15 18 22 29 37 44
breaking strength(N/mm) 20 27 33 40 53 67 80
Yield elongation(%) 12
breaking elongation(%) 700
3 Tear resistance(N) 93 125 156 187 249 311 374
4 Puncture resistance(N) 240 320 400 480 640 800 960
5 hstress crack resistance 300
6 carbon black              
  carbon black content(%) 2.0 ~ 3.0
carbon black dispersion carbon black dispersion(only near spherical agglomerates)for
  10different views 9 in categorise 1 0r 2 and 1 in category
7 Oxidative induction time(OIT)              
  standard OIT (min) 100
High pressure OIT (min) 400
8 Oven aging at 85 C              
  standard OIT-% retained after 90 days(%) 55
High pressure OIT-% retained alw 90 days(%) 80
9 UV Resistance              
  standard OIT retained after 1600hrs(%) 50
High pressure OIT retained after 1600hrs(%) 50
10 Low temperature impaci brinle at -70 C pass
11 permeability(g.cm/cm2.s.Pa) ≤1.0×10-13
12 Dimensional stability(%) ±2

Send your message to this supplier

*From:
*To:
avatar Mr. Jack Hu
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now

You Might Also Like

Contact Supplier

Diamond Member Since 2012

Suppliers with verified business licenses

Management System Certification
ISO 9001, ISO 14000
Terms of Payment
LC, T/T, D/P, Western Union
OEM/ODM Availability
Yes