Customization: | Available |
---|---|
Certification: | CE, ISO |
Surface: | Smooth Side |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
No. | Properties | Test Method | Test Value | |||||||
1 | Thickness(mm) | ASTM D5199 | 0.50 | 0.75 | 1.00 | 1.25 | 1.50 | 2.00 | 2.50 | 3.00 |
2 | Density (g/cm2) | ASTM D1505 | 0.939 | |||||||
3 | Tensile Strength(N/mm) | ASTM D6693 | 13 | 20 | 27 | 33 | 40 | 53 | 66 | 80 |
4 | Tensile Strength Elongation % | 800 | ||||||||
5 | 2% of the elastic modulus N/mm |
ASTM D5323 | 210 | 370 | 420 | 520 | 630 | 840 | 1050 | 1260 |
7 | Tear Resistance/N | ASTM D1004 | 50 | 70 | 100 | 120 | 150 | 200 | 250 | 300 |
8 | Puncture Resistance/N | ASTM D4833 | 120 | 190 | 250 | 310 | 370 | 500 | 620 | 750 |
9 | Multiaxis tensile Variable % | ASTM D5617 | 30 | |||||||
10 | Carbon Black | |||||||||
Carbon Black Content % | ASTM D1603 | 2.0-3.0 | ||||||||
Carbon Black Dispersion | ASTM D5596 | 10 9viewing area should fall in the first grade or second grade, third grade is not more than 1 | ||||||||
11 | Oxidative Induction Time(OIT) | |||||||||
Standard OIT/min | ASTM D3895 | 100 | ||||||||
High Pressure OIT/min | ASTM D5885 | 400 | ||||||||
12 | Oven Aging at 85°C | |||||||||
Standard OIT-% retained after 90 days | ASTM D3895 | 35 | ||||||||
High pressure OIT-% retained after 90 days | ASTM D5885 | 60 |